Carbide Milling Cutters SPIRON13-105-L/R11
coating type |
color |
hardness |
thickness |
CIF |
highest temperature |
TiN |
GOLDEN YELLOW |
2400 |
1~7 |
0.35 |
600 |
TiCN |
BLUISH-GREY |
3700 |
1~4 |
0.2 |
400 |
TiCN-MP |
RED-COPPER |
3200 |
1~4 |
0.2 |
400 |
TiALN |
PURPLISH-RED |
3300 |
1~4 |
0.4 |
800 |
CrN |
SLIVER |
1800 |
1~7 |
0.3 |
700 |
ACO |
DARK GREY |
4400 |
1~4 |
0.3 |
1100 |
TiCrN |
SLIVER/GOLD |
3000 |
1~7 |
0.4 |
600 |
XT |
GREY-BLACK |
4100 |
0.5~6 |
0.25 |
1100 |
DLC |
GREY-BLACK |
2000 |
1~3 |
0.1 |
400 |
MDT |
ROSE-PURPLE |
4000 |
1~4 |
0.25 |
800 |
With the improvement and improvement of the performance of the matrix material, the tool coating technology has achieved more rapid development, medium temperature chemical coating, columnar a-Al2O3 chemical coating, high-performance physical coating, new atomic coating, nanostructure coating. , yellow aluminum oxide chemical coating, white zirconium coating, high aluminum content TiAlN coating, TiSiN coating, CrSiN coating, AlCrSiN coating, TiBON coating and many other new coatings show a trend of diversification and serialization , so that new grades of cemented carbide materials emerge in an endless stream, which greatly improves the cutting performance of cemented carbide tools.